PRODUCTION OF GRAPHITE ELECTRODES BINDER FROM IRAQI ASPHALT

Main Article Content

Abdul Halim A.K. Mohammed
Hussaiin K.. Hussaiin
Tariiq M.. Naiieff

Abstract

Basrah crude oil Vacuum residue 773+ K with specific gravity 1.107 and 4.87wt. % sulfur, was
treated with hexane commercial fraction provided from Al-Taji Gas Company for preparing
deasphaltened oil(DAO)suitable for hydrotreating process.
Deasphaltening was carried out with 1h mixing time, 10ml:1g solvent to oil ratio and at room
temperature. Hexane deasphaltened oil was hydrotreated on presulfied commercial Co-Mo/ 2 3 g − Al O catalyst in a trickle bed reactor. The hydrotreating process was carried out at temperature 660 K,LHSV 1.3
h –1, H2/oil ratio 300 l/l and constant pressure of 4MPa. The hydrotreated product was distillated under vacuum distillation unit. It is found that the mixture of 75% of vacuum residue with 25% anthracene satisfies with requirements for graphite electrodes binder.

Article Details

Section

Articles

How to Cite

“PRODUCTION OF GRAPHITE ELECTRODES BINDER FROM IRAQI ASPHALT” (2006) Journal of Engineering, 12(01), pp. 219–226. doi:10.31026/j.eng.2006.01.16.

References

Gary,J.H., (1994), Petroleum Refining Technology and Economics, Third Edition

Hatano,H.and Suginobe,H.,Fuel,68(12),1503(1989).

Mohammed, A-H.A-H., Special Report of Al-Basil Company

Wagner, M.H., Jager, H., Letizia, I. and Wilhelmi, G., Fuel, 67(6),792(1988).

Wagner, M.H., Letizia, I., Gianini, S. and Wilhelmi, G., (1986),Int.Carbon Conference, Baden-Baden, 69

Similar Articles

You may also start an advanced similarity search for this article.